Matronics Email Lists Web Forum Interface to the Matronics Email Lists
|
View previous topic :: View next topic |
Author |
Message |
carlossa52(at)gmail.com Guest
|
Posted: Sat Jul 05, 2008 2:33 pm Post subject: metallurgical test |
|
|
Given a piece of aluminum 0.125 thick, triangular (square), small side 15 mm - does anybody know if it is possible to determine if it is actually 6061-T6?
An actual reference (as a specific lab name) would be great.
Thanks
Carlos
do not archive.
[quote][b]
| - The Matronics Zenith-List Email Forum - | | Use the List Feature Navigator to browse the many List utilities available such as the Email Subscriptions page, Archive Search & Download, 7-Day Browse, Chat, FAQ, Photoshare, and much more:
http://www.matronics.com/Navigator?Zenith-List |
|
|
|
Back to top |
|
|
bryanmmartin
Joined: 10 Jan 2006 Posts: 1018
|
Posted: Sat Jul 05, 2008 3:23 pm Post subject: metallurgical test |
|
|
It's certainly possible. The 6061 identifies the alloying elements
added to the aluminum and the T6 identifies the heat treat process. A
mass spectrometer would be one way to confirm the 6061 specification
and a hardness test could then probably verify the T6 specification.
I'm no expert but a good metallurgical lab should have no trouble with
this identification. Maybe a university lab would have the needed
equipment.
On Jul 5, 2008, at 6:29 PM, Carlos Sa wrote:
Quote: | Given a piece of aluminum 0.125 thick, triangular (square), small
side 15 mm - does anybody know if it is possible to determine if it
is actually 6061-T6?
An actual reference (as a specific lab name) would be great.
Thanks
Carlos
|
--
Bryan Martin
N61BM, CH 601 XL,
RAM Subaru, Stratus redrive.
do not archive.
| - The Matronics Zenith-List Email Forum - | | Use the List Feature Navigator to browse the many List utilities available such as the Email Subscriptions page, Archive Search & Download, 7-Day Browse, Chat, FAQ, Photoshare, and much more:
http://www.matronics.com/Navigator?Zenith-List |
|
_________________ --
Bryan Martin
N61BM, CH 601 XL, Stratus Subaru.
do not archive. |
|
Back to top |
|
|
carlossa52(at)gmail.com Guest
|
Posted: Sat Jul 05, 2008 8:49 pm Post subject: metallurgical test |
|
|
Right, I did find at least two labs that will do it, one of them a 5 minutes drive from home.
The 6061 specification requires about 1g of material (and costs $160).
The T6 test (tensile) requires samples 2" long for one lab case and 5" long for another ($70 per test).
Problem is, my sample is that small 0.125 thick, square triangle, small side 15 mm. A bigger sample destroys the subject of the testing.
I was hoping somebody on this list would have gone through this... I guess not, but thanks, anyway
Carlos
2008/7/5 Bryan Martin <bryanmmartin(at)comcast.net (bryanmmartin(at)comcast.net)>:
[quote] --> Zenith-List message posted by: Bryan Martin <bryanmmartin(at)comcast.net (bryanmmartin(at)comcast.net)>
It's certainly possible. The 6061 identifies the alloying elements added to the aluminum and the T6 identifies the heat treat process.
[b]
| - The Matronics Zenith-List Email Forum - | | Use the List Feature Navigator to browse the many List utilities available such as the Email Subscriptions page, Archive Search & Download, 7-Day Browse, Chat, FAQ, Photoshare, and much more:
http://www.matronics.com/Navigator?Zenith-List |
|
|
|
Back to top |
|
|
grs-pms(at)comcast.net Guest
|
Posted: Sat Jul 05, 2008 9:09 pm Post subject: metallurgical test |
|
|
Carlos:
Why not just buy some 6061-t6 with the proper certification? I'll bet that will be less expensive than testing what you have?
George
[quote] ---
| - The Matronics Zenith-List Email Forum - | | Use the List Feature Navigator to browse the many List utilities available such as the Email Subscriptions page, Archive Search & Download, 7-Day Browse, Chat, FAQ, Photoshare, and much more:
http://www.matronics.com/Navigator?Zenith-List |
|
|
|
Back to top |
|
|
carlossa52(at)gmail.com Guest
|
Posted: Sun Jul 06, 2008 5:19 am Post subject: metallurgical test |
|
|
Wellllllll, now I have to tell you this embarrassing story:
Some time ago I bought 6 pieces of aluminum 6061-T6 extrusion (1"x1"x0.125"), to be used on the spars.
All but one of these pieces had printed the mill's specifications on them (alloy, dimensions, mill name...).
While at the time I trusted the vendor was selling me the material I ordered, later I became disappointed with their services. I am now concerned about the composition of the unlabeled extrusion.
Further, the parts have been primed and assembled (as in "riveted"), so I don't know which one is the "suspect". I need to verify the six of them to be sure.
The alternative is to trash the spars, which includes disassembling a partially riveted outboard wing.
As you see, the lab test is expensive, but it is the cheaper (effort-wise) alternative at hand.
Carlos
CH601-HD, plans
2008/7/6 George Swinford <grs-pms(at)comcast.net (grs-pms(at)comcast.net)>:
[quote] Carlos:
Why not just buy some 6061-t6 with the proper certification? I'll bet that will be less expensive than testing what you have?
George
[b]
| - The Matronics Zenith-List Email Forum - | | Use the List Feature Navigator to browse the many List utilities available such as the Email Subscriptions page, Archive Search & Download, 7-Day Browse, Chat, FAQ, Photoshare, and much more:
http://www.matronics.com/Navigator?Zenith-List |
|
|
|
Back to top |
|
|
larry(at)macsmachine.com Guest
|
Posted: Sun Jul 06, 2008 6:21 am Post subject: metallurgical test |
|
|
Carlos,
I'd order another piece from them, requesting certification of the
6061-T6 pieces sent and test what they send you.
Test against the known values for 6061-T6. That's as close as it gets.
Larry McFarland 601HDS at www.macsmachine.com
do not archive
Carlos Sa wrote:
Quote: | Wellllllll, now I have to tell you this embarrassing story:
Some time ago I bought 6 pieces of aluminum 6061-T6 extrusion
(1"x1"x0.125"), to be used on the spars.
All but one of these pieces had printed the mill's specifications on
them (alloy, dimensions, mill name...).
While at the time I trusted the vendor was selling me the material I
ordered, later I became disappointed with their services. I am now
concerned about the composition of the unlabeled extrusion.
*
*
|
| - The Matronics Zenith-List Email Forum - | | Use the List Feature Navigator to browse the many List utilities available such as the Email Subscriptions page, Archive Search & Download, 7-Day Browse, Chat, FAQ, Photoshare, and much more:
http://www.matronics.com/Navigator?Zenith-List |
|
|
|
Back to top |
|
|
carlossa52(at)gmail.com Guest
|
Posted: Sun Jul 06, 2008 6:44 am Post subject: metallurgical test |
|
|
But Larry, how would that prove that all the material I bought from them in the past - and are now part of my spars - are actually 6061-T6?
What I am suggesting is that, when I bought them, someone in the warehouse pulled one extrusion out of the wrong shelf. (Of course I am hoping it is simply an honest-to-goodness piece of 6061-T6, just unlabeled).
The only way to make sure is to cut samples form the extrusions and testing them (BTW, I got clearance from ZAC for cutting samples with these dimensions from the spars).
Thanks for the input
Carlos
2008/7/6 LarryMcFarland <larry(at)macsmachine.com (larry(at)macsmachine.com)>:
[quote] --> Zenith-List message posted by: LarryMcFarland <larry(at)macsmachine.com (larry(at)macsmachine.com)>
Carlos,
I'd order another piece from them, requesting certification of the 6061-T6 pieces sent and test what they send you.
Test against the known values for 6061-T6. That's as close as it gets.
Larry McFarland 601HDS at www.macsmachine.com
do not archive
Carlos Sa wrote:
Quote: | Wellllllll, now I have to tell you this embarrassing story:
Some time ago I bought 6 pieces of aluminum 6061-T6 extrusion (1"x1"x0.125"), to be used on the spars.
All but one of these pieces had printed the mill's specifications on them (alloy, dimensions, mill name...).
While at the time I trusted the vendor was selling me the material I ordered, later I became disappointed with their services. I am now concerned about the composition of the unlabeled extrusion.
| [b]
| - The Matronics Zenith-List Email Forum - | | Use the List Feature Navigator to browse the many List utilities available such as the Email Subscriptions page, Archive Search & Download, 7-Day Browse, Chat, FAQ, Photoshare, and much more:
http://www.matronics.com/Navigator?Zenith-List |
|
|
|
Back to top |
|
|
carlossa52(at)gmail.com Guest
|
Posted: Sun Jul 06, 2008 9:13 am Post subject: metallurgical test |
|
|
In case somebody ever finds him/herself in the same predicament, I found a tool made for just this situation:
http://www.worldoftest.com/pdf/Webster.pdf
Questions is, does it cost more than an HD wing?
I sent them a note, stay tuned (if you care).
Carlos
2008/7/6 Carlos Sa <carlossa52(at)gmail.com (carlossa52(at)gmail.com)>:
[quote] Wellllllll, now I have to tell you this embarrassing story:
Some time ago I bought 6 pieces of aluminum 6061-T6 extrusion (1"x1"x0.125"), to be used on the spars.
All but one of these pieces had printed the mill's specifications on them (alloy, dimensions, mill name...).
While at the time I trusted the vendor was selling me the material I ordered, later I became disappointed with their services. I am now concerned about the composition of the unlabeled extrusion.
Further, the parts have been primed and assembled (as in "riveted"), so I don't know which one is the "suspect". I need to verify the six of them to be sure.
The alternative is to trash the spars, which includes disassembling a partially riveted outboard wing.
As you see, the lab test is expensive, but it is the cheaper (effort-wise) alternative at hand.
Carlos
CH601-HD, plans
[b]
| - The Matronics Zenith-List Email Forum - | | Use the List Feature Navigator to browse the many List utilities available such as the Email Subscriptions page, Archive Search & Download, 7-Day Browse, Chat, FAQ, Photoshare, and much more:
http://www.matronics.com/Navigator?Zenith-List |
|
|
|
Back to top |
|
|
Brady
Joined: 26 May 2008 Posts: 182 Location: Poulsbo, WA
|
Posted: Sun Jul 06, 2008 12:09 pm Post subject: Re: metallurgical test |
|
|
Carlos,
I had a friend in a similar situation.
Fortunately he is a structural engineer at the navy ship yard and had access to all of the facilities assets in this discipline.
The test that he settled on was a hardness test.
His thinking was that if the aluminum was not 6061 t6 it was a 3xxx series and would be way off. so using a known 6061 t6 sample he got a base line measurement and then tested the suspect sample.
He was surprised to find that not only was he correct in his theory but also that the difference is staggering!
I have been able to simulate this test with out the expensive machinery by using an automatic center punch. Punch a piece of 6061 T6 and notice the divot left by the tool. Then punch the sample you suspect. If there is no noticeable difference the chances are excellent that you have the same alloy.
If you have a substandard alloy the divot will be noticeably deeper.
Obviously this method is not completely accurate or totally reliable but it is enough to tell you if you are with in the extremes.
Hope this helps,
Brady
| - The Matronics Zenith-List Email Forum - | | Use the List Feature Navigator to browse the many List utilities available such as the Email Subscriptions page, Archive Search & Download, 7-Day Browse, Chat, FAQ, Photoshare, and much more:
http://www.matronics.com/Navigator?Zenith-List |
|
_________________ Brady McCormick
Poulsbo, WA
www.magnificentmachine.com |
|
Back to top |
|
|
bcchurch
Joined: 10 Dec 2007 Posts: 25 Location: Racine, WI
|
Posted: Tue Jul 08, 2008 5:17 pm Post subject: Re: metallurgical test |
|
|
Carlos,
I'm a materials engineer and would like to offer my advice. What you should do is confirm a) chemical composition and b) mechanical properties. Chemical composition can be done easily via ICP or OES and your sample is definitely large enough for either test. The price you listed seemed reasonable - just make sure the lab gives you actual results and not just a "meets 6061" statement. You want to know actual weight percent of silicon, magnesium, iron, manganese, etc.
The more difficult issue for you is mechanical properties.
The 6061-T6 spec calls out yield, tensile, and elongation which are all determined via a standard tensile test. As you already know, the size of your sample is too small to perform a tensile test. My opinion is that you should ask for hardness tests on your unknown sample as well as a known 6061-T6 of the same thickness. Hardness is not the ideal way to do this - but given your situation it's the best-possible way.
If chemistry checks out, then go ahead with the hardness tests. If the hardness results of the known and unknown are similar (I very much doubt they will be exactly equal) then I'd say you're good to assume your 6061 is indeed T6. I'd also double check the hardness results of both known and unknown samples versus "handbook" values for 6061-T6 for added comfort. The hardness tests would not be definitive proof - but it would be good enough for me if I were in your shoes.
Hope this helps. Feel free to email me at bcchurch-at-yahoo.com if you have any questions.
Regards,
Ben
| - The Matronics Zenith-List Email Forum - | | Use the List Feature Navigator to browse the many List utilities available such as the Email Subscriptions page, Archive Search & Download, 7-Day Browse, Chat, FAQ, Photoshare, and much more:
http://www.matronics.com/Navigator?Zenith-List |
|
_________________ Ben Church
CH801
Racine, WI |
|
Back to top |
|
|
|
|
You cannot post new topics in this forum You cannot reply to topics in this forum You cannot edit your posts in this forum You cannot delete your posts in this forum You cannot vote in polls in this forum You cannot attach files in this forum You can download files in this forum
|